Anatase
Anatase

Zircon
Zircon



ADD
Compare
X
Anatase
X
Zircon

Anatase and Zircon Physical Properties

Add ⊕
1 Physical Properties
1.1 Tenacity
Brittle
Brittle
1.2 Solubility
Not Available
insoluble
1.3 Durability
Not Available
Not Available
1.4 Specific Gravity
3.82-3.973.93-4.73
Amber
1 7.18
1.5 Fracture
Subconchoidal, Conchoidal, Brittle, ConchoidalArthur Thomas, Gemstones (2009)
Conchoidal, Uneven, ConchoidalArthur Thomas, Gemstones (2009)
1.6 Cleavage
Perfect on [001] and [011]
{110} and {111}
1.7 Mohs Hardness
5.5-67.5
Amber
2 10
1.8 Chemical Composition
TiO 2Michael O’Donoghue , Gems, Sixth edition (2006) More from other references
ZrSiO4

Anatase and Zircon Chemical Formula

While comparing Anatase and Zircon physical properties, the important data you should know is its chemical composition. Since chemical formula defines the molecular structure of the crystal, most of the physical properties like color, tenacity, solubility are governed by Anatase and Zircon chemical formula.

  • Chemical formula of Anatase- TiO 2Michael O’Donoghue , Gems, Sixth edition (2006) More from other references
  • Chemical formula of Zircon- ZrSiO4

Anatase and Zircon Specific Gravity

Another important criteria for qualitative analysis of gemstones is Anatase and Zircon Specific gravity. Specific gravity is the relative density of a gemstone compared with respect to density of water. Gemologists use Anatase and Zircon Optical Properties during the identification of gemstone. Specific gravity of Anatase is 3.93-4.73 whereas that of Zircon is 3.93-4.73.